Technical Data :

 

Items

ZD-650

(SG-9)

ZD-700

(SG-8)

ZD-800

(SG-7)

Testing Method and Standard

GB/T5761

 

Appearance

 

White powders

 

White powders

 

White powders

 

Vissual inspection

 

Adhesion Number / (mL/g)

 

71-73

 

86-73

 

86-95

 

GB/T3401

 

K value

 

54-55

 

55-59

 

60-62

 

GB/T3401

 

Numbers of impurities particles ≤

 

30

 

30

 

30

 

GB/T 9348

 

Total volatile content / ﹪≤

 

0.4

 

0.4

 

0.4

 

GB/T 2914

Residue after sieving /%

250um pore ≤

 

2.0

 

2.0

 

2.0

 

 

GB/T2916

63um

pore ≥

 

95

 

95

 

95

Apparent Density / (g/mL)≥

 

0.45

 

0.45

 

0.45

 

GB/T20022

“ Fish eye ”numbers /

( 个 / 400cm 2 ) ≤

 

30

 

30

 

30

 

GB/T 4611

plasticizer absorption for 100g resin / g ≥

 

12

 

12

 

12

 

GB/T 3400

Whiteness ≥

( 16 0 ℃ ,10min)/ %

 

75

 

75

 

75

 

GB/T15595

Vinyl monermer content /(ug/g) ≤

 

5

 

5

 

5

 

GB/T4615

 

   

Storage:

Store in dry places (less than 25 ℃ ), the shelf life if stored in the above conditions will be at least 12 months from the date of delivery.

Packing:

Packed in polypropylene woven bag with polypropylene plastic inner bag. Weight: 25 kg/bag.

 

 

 

 